GoldFlex Technical Data
Property |
Test/Method |
Typical Value |
Film Structure - Recoil™ Technology |
Fusion Coating - Proprietary Polymer Blend |
Weight (GSM) |
ASTM D5261 |
440 |
Nominal Thickness (Mils) |
ASTM D1777 |
26 |
Hydrostatic Resistance (PSI) |
ASTM D751 |
370 |
Breaking Strength (lbs) |
ASTM D751 |
Machine Direction 450 | Cross Direction 425 |
Tear Resistance (lbs) |
ASTM D751 |
Machine Direction 78 | Cross Direction 74 |
Puncture Resistance (lbs) |
ASTM D751 |
190 |
Bursting strength (Ball burst) (PSI) |
ASTM D751 |
710 |
Low Temperature Flexibility |
ASTM D2136 |
-50 °C |
Accelerated UV Weathering |
ASTM G154 |
> 90% @ 2000 Hours† |
All values are ± 10%. †QUV A-340 lamps 8 hrs UV @ 60° C, 4 hrs condensation @ 40°. The test data is based on an average taken over several production runs and should not be considered or interpreted as minimum or maximum values. Values are typical data and not limiting specifications.